Element | |||
---|---|---|---|
Cu(1,2) | Cr | Zr | |
Min (%) | 0.5 | 0.03 | |
Max (%) | Rem | 1.5 | 0.3 |
Form | Tensile Strength In Mpa | Elongation In % | Rockwell Hardness in B Scale-HRB |
---|---|---|---|
Rod | >360 | >10 | >68 |
Flat Products | >360 | >10 | >68 |
SC Ring | >360 | >15 | >65 |
Wheel | - | - | >68 |
Tube | - | - | >68 |
Block | - | - | >68 |
Melting Point – Liquidus °C | 1080 |
Melting Point – Solidus °C | 1070 |
Density lb/cu in. at 20°C | 0.321 |
Specific Gravity | 8.89 |
Electrical Conductivity% IACS at 20°C | 80 |
Thermal Conductivity Btu/ sq ft/ ft hr/ °F at 20°C | 187 |
Coefficient of Thermal Expansion 20-100 10⁻⁶ per °F (20 – 100°F) | 9.5 |
Modulus of Elasticity in Tension ksi | 17000 |
Treatment | Minimum* | Maximum* | Value* | Time** | |
---|---|---|---|---|---|
Solution Treatment | 0.5 | ||||
Precipitation Treatment | 427 | 3 | |||
Annealing | 982 | 1010 | |||
Hot Treatment | 815 | 927 | |||
* Temperature is measured in Celsius. ** Time is measured in minutes. |
Technique | Stability |
---|---|
Machinability Rating | 20 |
Form | Description |
---|---|
Rod | Hot Extruded & Cold Drawn Copper Rod |
Flat | Hot Extruded & Cold Drawn Copper (Bar, Strips) |
Profile | Hot Extruded & Cold Drawn Copper Cut to length |
Wheel | Forged and Machined |
Tube | Hot Extruded Tube & Machined |
Block | Forged and Machined |
Ring | Forged, Rolled and Machined |
Product Category | Product | Reason |
---|---|---|
Electrical | Connectors | Electrical Connectors Electrical Conductivity, Moderate Strength, Thermal Conductivity |
Contacts | Electrical Conductivity, Moderate Strength, Thermal Conductivity | |
Electric Motor and Generator Components | Electrical Conductivity, Thermal Conductivity | |
Electrical Conductors Requiring Greater Strength than Copper | Electrical Conductivity, Moderate Strength | |
Electrical Connectors | Electrical Conductivity, Thermal Conductivity, Heat Treatable, Moderate Strength | |
Electron Tube Grid Side Rods | Electrical Conductivity, Moderate Strength, Retains Strength at High Temperatures | |
Parts for Electronic Devices | Electrical Conductivity, Moderate Strength, Thermal Conductivity | |
Semi-Conductor Bases | Electrical Conductivity, Moderate Strength | |
Switch Contacts | Electrical Conductivity, Thermal Conductivity | |
Switch Gears | Electrical Conductivity, Moderate Strength, Thermal Conductivity | |
Thermal Conductors Requiring Greater Strength than Copper | Electrical Conductivity, Moderate Strength | |
Industrial | Resistance Welding Machine Electrodes | Electrical Conductivity, Thermal Conductivity |
Seam Welding Wheels | Electrical Conductivity, Thermal Conductivity | |
Spot Welding Tips | Electrical Conductivity, Thermal Conductivity | |
Short Circuit Ring | Electrical Conductivity, Thermal Conductivity |
Copyrights © 2019 Modison Copper Pvt Ltd | All Rights Reserved.